[1] R. Riedel, A. Kienzle, W. Dressler, L. Ruwisch, J. Bill, F. Aldinger, A silicoboron carbonitride ceramic stable to 2,000 degrees C, Nature 382(6594) (1996) 796-798.
[2] M. Christ, G. Thurn, M. Weinmann, J. Bill, F. Aldinger, High-temperature mechanical properties of Si-B-C-N-precursor-derived amorphous ceramics and the applicability of deformation models developed for metallic glasses, J. Am. Ceram. Soc. 83(12) (2000) 3025-3032.
[3] N.V.R. Kumar, S. Prinz, Y. Cai, A. Zimmermann, F. Aldinger, F. Berger, K. Muller, Crystallization and creep behavior of Si-B-C-N ceramics, Acta Mater. 53(17) (2005) 4567-4578.
[4] H. Schmidt, W. Gruber, G. Borchardt, P. Gerstel, A. Muller, N. Bunjes, Coarsening of nano-crystalline SiC in amorphous Si-B-C-N, J. Eur. Ceram. Soc. 25(2-3) (2005) 227-231.
[5] Z. Yang, D. Jia, X. Duan, K. Sun, Y. Zhou, Effect of Si/C ratio and their content on the microstructure and properties of Si-B-C-N Ceramics prepared by spark plasma sintering techniques, Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing 528(4-5) (2011) 1944-1948.
[6] F. Aldinger, M. Weinmann, J. Bill, Precursor-derived Si-B-C-N ceramics, Pure and Applied Chemistry 70(2) (1998) 439-448.
[7] D. Jia, B. Liang, Z. Yang, Y. Zhou, Metastable Si-B-C-N ceramics and their matrix composites developed by inorganic route based on mechanical alloying: Fabrication, microstructures, properties and their relevant basic scientific issues, Progress in Materials Science 98 (2018) 1-67.
[8] A. Evans, Perspective on the Development of High-Toughness Ceramics, Journal of the American Ceramic Society 73 (2005) 187-206.
[9] T. Besmann, B. Sheldon, R. Lowden, D. Stinton, Vapor-Phase Fabrication and Properties of Continuous-Filament Ceramic Composites, Science (New York, N.Y.) 253 (1991) 1104-9.
[10] H. Zhao, L.X. Chen, X.G. Luan, X.F. Zhang, J. Yun, T.T. Xu, Synthesis, pyrolysis of a novel liquid SiBCN ceramic precursor and its application in ceramic matrix composites, J. Eur. Ceram. Soc. 37(4) (2017) 1321-1329.
[11] Y.-L. Li, E. Kroke, R. Riedel, C. Fasel, C. Gervais, F. Babonneau, Thermal Cross-Linking and Pyrolytic Conversion of Poly(Ureamethylvinyl)Silazanes to Silicon-Based Ceramics, Applied Organometallic Chemistry 15 (2001) 820-832.
[12] S. Yajima, T. Shishido, H. Kayano, K. Okamura, M. Omori, J. Hayashi, SiC sintered bodies with three-dimensional polycarbosilane as binder, Nature 264(5583) (1976) 238-239.
[13] R. D'Elia, G. Dusserre, S. Del-Confetto, N. Eberling-Fux, C. Descamps, T. Cutard, Cure kinetics of a polysilazane system: Experimental characterization and numerical modelling, European Polymer Journal 76 (2016) 40-52.
[14] S.H. Lee, M. Weinmann, F. Aldinger, Processing and properties of C/Si-B-C-N fiber-reinforced ceramic matrix composites prepared by precursor impregnation and pyrolysis, Acta Mater. 56(7) (2008) 1529-1538.
[15] Q. Ding, D. Ni, Z. Wang, H. Zhong, H. Wang, H. Zhou, Y. Kan, S. Dong, 3D Cf/SiBCN composites prepared by an improved polymer infiltration and pyrolysis, J Adv Ceram 7(3) (2018) 266-275.
[16] H. Zhong, Z. Wang, H. Zhou, D. Ni, Y. Kan, Y. Ding, S. Dong, Properties and microstructure evolution of Cf/SiC composites fabricated by polymer impregnation and pyrolysis (PIP) with liquid polycarbosilane, Ceramics International 43(10) (2017) 7387-7392.
[17] Z. Yu, L. Yang, H. Min, P. Zhang, C. Zhou, R. Riedel, Single-source-precursor synthesis of high temperature stable SiC/C/Fe nanocomposites from a processable hyperbranched polyferrocenylcarbosilane with high ceramic yield, J. Mater. Chem. C 2(6) (2014) 1057-1067.